Wet film to dry film: the formula
Wet thickness includes liquid that can leave during drying. The solids-by-volume fraction links the applied wet film thickness (WFT) to the theoretical dry film thickness (DFT). The converter assumes the added thinner contributes no solids and that volumes are additive.
- Effective solids fraction = (volume solids ÷ 100) ÷ (1 + thinner % ÷ 100)
- DFT = WFT × effective solids fraction
- WFT = DFT ÷ effective solids fraction
Use the solids value for the correctly mixed coating before the extra thinner. If a data sheet already gives the reduced mixture's solids by volume, use that value and set added thinner to zero—otherwise thinning would be counted twice.
A single reading—or both ends of a range
For a wet film comb, use the highest wetted notch and next higher unwetted notch as the two bounds. The converter carries that interval through the calculation rather than pretending the midpoint is an exact measurement. In the reverse direction, enter a specified dry range to estimate the corresponding wet application range.
| Wet film | Volume solids | Theoretical dry film |
|---|---|---|
| 200 µm | 60% | 120 µm |
| 250 µm | 60% | 150 µm |
| 8–10 mil | 65% | 5.2–6.5 mil |
| 150 µm | 100% | 150 µm |
Why thinning changes the result
Thinner adds wet volume without adding coating solids. For the same dry target, more wet thickness is needed; for the same wet reading, the estimated dry thickness is lower. Our thinner percentage is relative to the original mixed coating volume, not the total after adding thinner.
A 100 µm dry target with 60% solids and 10% added thinner needs about 183.33 µm wet. Without that thinner, the estimate is 166.67 µm wet. These are theoretical values; do not round a project tolerance into a pass/fail decision.
Frequently asked questions
How do you convert wet film thickness to dry film thickness?
Without thinning, multiply wet film thickness by the solids-by-volume fraction. A 200 µm wet film at 60% volume solids gives a theoretical 120 µm dry film.
How does added thinner change the conversion?
For thinner with no solids, divide the original solids fraction by 1 plus the added-thinner fraction. Here, 10% thinner means 0.1 liter added to 1 liter of mixed coating, not 10% of the final mixture.
Can I use solids by weight?
No. Use solids by volume from the technical data sheet for the coating as mixed before the extra thinner. Solids by weight is not interchangeable with solids by volume.
Can I convert a wet film comb reading range?
Yes. Enter the highest wetted notch as the lower bound and the next higher unwetted notch as the upper bound. The result is a theoretical dry thickness range, not a precise reading.
Does this replace a dry film thickness measurement?
No. This is a theoretical estimate. Surface texture, application and cure can affect actual results. Follow the product data sheet and project specification, and verify dry film thickness after cure.
Formula and measurement reference
DeFelsko: wet film measurement and WFT/DFT formulas explains solids by volume, added reducer and interpreting comb readings. For unit-only conversions, use our mils to mm converter.